The fundamental basis for mechanistic understanding and modeling of SCC remains in question for many systems. Specific mechanisms controlling SCC can vary with changes in alloy characteristics, applied/residual stress or environmental conditions. The local crack electrochemistry, crack-tip mechanics and material metallurgy are the main factors controlling crack growth. These localized properties are difficult or impossible to measure in active cracks. Nevertheless, it is essential to quantitatively interrogate these crack-tip conditions if mechanistic understanding is to be obtained. A major recent advance has been the ability to investigate SCC cracks and crack tips using high-resolution ATEM techniques. ATEM enables the characterization of SCC cracks including trapped tip solution chemistries, corrosion product/film compositions and structures, and elemental composition gradients and defect microstructures along the crack walls and at the crack tip. A wide variety of methods for imaging and analyses at resolutions down to the atomic level can be used to examine the crack and corrosion film characteristics. Surface films and reaction layers have been examined by cross-sectional TEM techniques, but little work had been conducted on environmentally induced internal cracks until that of Lewis and co-workers [1-3] and the current authors [4-17]. This capability combined with modern ATEM techniques has enabled exciting new insights into corrosion processes occurring at buried interfaces and is being used to identify mechanisms controlling IGSCC in boiling water reactor (BWR) and pressurized water reactor (PWR) components. The objective of this paper is to summarize certain results focused on IGSCC of Fe- base and Ni-base stainless alloys in high-temperature water environments. Representative crack-tip examples will be shown to illustrate specific aspects that are characteristic of SCC in the material/environment combinations. Differences and similarities in crack-tip structures- chemistries will be highlighted comparing Fe-base 316/304SS to Ni-base alloy 600/182 and for tests in oxidizing versus hydrogenated water environments.
Revised: September 6, 2011 |
Published: April 5, 2010
Citation
Bruemmer S.M., and L.E. Thomas. 2010.Insights into Stress Corrosion Cracking Mechanisms from High-Resolution Measurements of Crack-Tip Structures and Compositions. In Materials Research Society Spring Meeting, Actinides V: Basic Science, Applications and Techniology, April 6-8, 2010, San Francisco, California, edited by JK Gibson, 1264, 159-172; Paper No. 1264-BB01-09. Warrendale, Pennsylvania:Materials Research Society.PNNL-SA-72019.doi:10.1557/PROC-1264-BB01-09