August 1, 2012
Report

Assessment of Weld Overlays for Mitigating Primary Water Stress Corrosion Cracking at Nickel Alloy Butt Welds in Piping Systems Approved for Leak-Before-Break

Abstract

This TLR provides an assessment of weld overlays as a mitigation strategy for PWSCC, and includes an assessment of the WOL-related inspection requirements of Code Case N-770-1, as conditioned in ยง50.55a.

Revised: January 25, 2013 | Published: August 1, 2012

Citation

Sullivan E.J., E.J. Sullivan, and M.T. Anderson. 2012. Assessment of Weld Overlays for Mitigating Primary Water Stress Corrosion Cracking at Nickel Alloy Butt Welds in Piping Systems Approved for Leak-Before-Break Richland, WA: Pacific Northwest National Laboratory.