Two further failed thermal creep pressurized tubes of V-4Cr-4Ti tested at 700 and 800 degrees C have been examined using optical microscopy and transmission electron microscopy in order to understand failure and creep mechanisms. These conditions represent lower stress states than were previously examined. Creep deformation at lower stress is shown to be controlled by sub-boundary formation and mis-orientation between sub-grains arising from climb of dislocations within the boundary.